SUKO-1

Farashin PTFE

Manufar hatimin mai shine don samar da hatimi tsakanin crankshaft mai juyawa da waje.Hatimin mai na gargajiya ya ƙunshi mahalli na ƙarfe wanda ke ɗaukar leɓe mai ƙarfi kuma yana ba da aikin rufewa.Leben hatimin hatimin mai galibi ana kera shi ne da kayan elastomer, kuma yana cikin hulɗa da saman shingen jujjuyawar.Ta haka, ana matse leɓe a saman shaft ta hanyar zoben bazara.Sakamakon motsin jujjuyawar, akwai tazarar rufewa kusan.1 µm a gefen lebe.Man zai iya shiga wannan rata, wanda ke yin amfani da man shafawa ga leɓen rufewa.

Farashin PTFE

Ci gaba da ci gaba a ƙirar injin yana haifar da ƙarin buƙatu akan wannan nau'in hatimin mai.Maɗaukakin injunan saurin injuna da yanayin mai, tsayin tazara tsakanin canje-canjen mai da man shafawa tare da ƙari na zamani waɗanda ke da ƙarfi tare da kayan rufewa suna buƙatar sabbin mafita mai dorewa.Abu na gaba mai hatimin mai suna POLYTETRAFLUOROETHYLENE ko kuma kawai PTFE.Wannan abu na roba an fi saninsa a ƙarƙashin sunan kasuwanci polymer.

Ƙananan juzu'i da mafi ƙarancin amfani da wutar lantarki sune fa'idodin fa'idodin da hatimin mai na PTFE ke bayarwa.Ana iya amfani da waɗannan hatimin ba tare da matsala ba kuma tare da bushewar aiki ko rashin isasshen man shafawa.Abubuwan thermal Properties, tare da kewayon aiki na -130°C zuwa +200°C, ba su da bambanci.Bugu da ƙari, PTFE ana nuna shi ta babban juriya na sinadarai da ƙananan karfin juriya bayan tsayawa.

Lokacin da zafi, PTFE yayi ƙoƙarin komawa zuwa asalin sa.A wasu kalmomi: Kayan yana "tunani" yanayin asali ne.Wannan al'amari an san shi da tasirin ƙwaƙwalwar filastik, kuma yana ba da izinin gina hatimi ba tare da tsinkayar bazara ba.Lokacin kera, leɓen rufewa yana siffata azaman zobe mai lebur, wanda aka ƙera shi zuwa zoben ƙarfafawa.Yayin haɗa kan sandar, leɓen hatimin farko na lebur yana faɗaɗa kuma ya ninka don dacewa da diamita na shaft.Da zarar leben da ke rufewa ya yi zafi yayin aikin injin, yana ƙoƙarin komawa ga ainihin siffarsa.

Gidan waje an yi shi da bakin karfe.Ring O na fluoroelastomer yana tabbatar da mafi kyawun hatimi a tsaye.Diamita na ciki yana da kyau sosai tare da diamita na waje.Ainihin leɓen rufewa an yi shi da juriya mai ƙarfi da ƙarancin gogayya PTFE.Ƙarin hatimin ƙura (leben roba ko tsiri mai ji) yana ba da shinge mai tasiri daga gurɓataccen ƙwayar cuta.


Lokacin aikawa: Mayu-04-2020